Haɗin sinadarai na bututun ƙarfe na ASTM A333 Gr.6, Halayen Inji da Juriyar Girma

ASTM A333 Gr.6 Karfe bututu

Bukatun Sinadaran da ake buƙata,%,

C: ≤0.30

Mn: 0.29-1.06

P: ≤0.025

S: ≤0.025

Si: ≥0.10

Ni: ≤0.40

Cr: ≤0.30

Cu: ≤0.40

V: ≤0.08

Lambar lamba: ≤0.02

Wata: ≤0.12

*Ana iya ƙara yawan sinadarin manganese da kashi 0.05% ga kowace raguwar kashi 0.01% na sinadarin carbon har zuwa kashi 1.35%.

**Ana iya ƙara yawan sinadarin Niobium zuwa 0.05% don nazarin narkewa da kuma 0.06% don nazarin samfurin da aka gama.

Bukatun maganin zafi:

1. Daidaita yanayin zafi sama da 815°C.

2. A daidaita zafin da ke sama da 815°C, sannan a rage zafi.

3. Zafi ya yi tsakanin 845 zuwa 945°C, sannan a sanyaya a cikin tanda sama da 845°C (don bututun da ba su da sumul kawai).

4. An yi masa injina sannan a rage zafi kamar yadda aka bayyana a sama a Mataki na 3.

5. An taurare sannan aka rage zafi sama da 815°C.

Bukatun aikin injiniya:

Ƙarfin samarwa: ≥240Mpa

Ƙarfin tensile: ≥415Mpa

Ƙarawa:

Samfuri

A333 GR.6

Tsaye

Mai wucewa

Mafi ƙarancin ƙimar da'ira ta yau da kullunsamfurin ko ƙaramin samfurin sikelin tare da nisan alama na 4D

22

12

Samfuran murabba'i masu kauri na bango na inci 5/16 (7.94 mm) ko fiye, da kuma duk ƙananan samfuran da aka gwada a cikicikakken giciye a inci 2 (mm 50)alamomi

30

16.5

Samfuran murabba'i har zuwa inci 5/16 (7.94 mm) kauri bango a inci 2 (50 mm) nisan alama (faɗin samfurin 1/2 inci, 12.7 mm)

A

A

 

A Ba da damar rage tsawon tsayi da kashi 1.5% da kuma rage tsawon tsayi da kashi 1.0% ga kowane kauri na 1/32 inci (0.79 mm) har zuwa inci 5/16 (7.94 mm) daga ƙimar tsawaita da aka lissafa a sama.

Gwajin Tasiri

Zafin Gwaji: -45°C
Lokacin da aka yi amfani da ƙananan samfuran tasirin Charpy kuma faɗin ƙimar samfurin ya ƙasa da kashi 80% na ainihin kauri na kayan, ya kamata a yi amfani da ƙaramin zafin gwajin tasiri kamar yadda aka ƙididdige a cikin Tebur 6 na ƙayyadaddun ASTM A333.

Samfura, mm

Matsakaicin matsakaicin samfura uku

Mafi ƙarancin ƙimar akane

of samfuran uku

10 × 10

18

14

10 × 7.5

14

11

10 × 6.67

12

9

10 × 5

9

7

10 × 3.33

7

4

10 × 2.5

5

4

Ya kamata a gwada bututun ƙarfe ta hanyar hydrostatic ko kuma ba ta hanyar lalata su ba (eddy current ko ultrasonic) a kan reshe-reshe.

Juriyar diamita na waje na bututun ƙarfe:

 

Diamita na waje, mm

haƙuri mai kyau, mm

haƙuri mara kyau, mm

10.3-48.3

0.4

0.4

48.3D≤114.3

0.8

0.8

114.3D≤219.10

1.6

0.8

219.1D≤457.2

2.4

0.8

457.2D≤660

3.2

0.8

660D≤864

4.0

0.8

864D≤1219

4.8

0.8

 

Juriyar kauri na bututun ƙarfe:

Duk wani maki ba zai zama ƙasa da kashi 12.5% ​​na kauri na bango ba. Idan an tsara mafi ƙarancin kauri na bango, babu wani maki da zai zama ƙasa da kauri na bango da ake buƙata.